Enhance concrete durability with high tensile reinforcement.Alkali-resistant and non-corrosiveReinforces unsupported spans and cantilevered sectionsPrevents surface ghosting with proper placement
| Color | Off White |
| Specific Gravity | 1.17 |
| Density | 1,762 - 2,082 kg/m3 |
| Packaging | 0.45 kg, 3.6 kg, 18.1 kg |
| Fiber Length | 6 mm |
| Filament Diameter | 12-15 μm |
| Decomposition Temperature | 330º C |
| Elastic Modulus | >5.5 GPa |
| Typical Dosage | 20 grams per 50 lb of concrete mix |
| Fiber Count | 680,000,000 fibers/kg |
Enhance concrete durability with high tensile reinforcement.Alkali-resistant and non-corrosiveReinforces unsupported spans and cantilevered sectionsPrevents surface ghosting with proper placement
Enhance concrete durability with secondary reinforcement.Eliminates plastic shrinkage crackingAlkali resistant and non-corrosiveInsoluble in waterNo fiber protrusion for easy finishingHigh impact resistance
Provides primary reinforcement and enhances concrete durability and performance.High tensile strengthAlkali and corrosion-resistantUse 3% by weight of the total mix0.68-0.79 kg per bagAdd fibers later in mixing
Enhance concrete strength and crack and abrasion resistance through a multi-directional PVA-fiber network.Disperse as monofilamentsVisibility varies by size1% PVA 100 and 0.75% PVA 15 blend recommendedPotential mix stiffening at high doses.
| Product | Color | Specific Gravity | Density | Packaging | Fiber Length | Filament Diameter | Decomposition Temperature | Elastic Modulus | Typical Dosage | Fiber Count |
|---|---|---|---|---|---|---|---|---|---|---|
| Alkali Resistant AR Glass Scrim | - | - | - | - | - | - | - | - | - | - |
| Acrylic Fiber AC50 | Off White | 1.17 | 1,762 - 2,082 kg/m3 | 0.45 kg, 3.6 kg, 18.1 kg | 6 mm | 12-15 μm | 330º C | >5.5 GPa | 20 grams per 50 lb of concrete mix | 680,000,000 fibers/kg |
| Alkali Resistant AR Glass Fiber | - | - | - | - | - | - | - | - | - | - |
| PVA (Polyvinyl Alcohol) Fiber | - | - | - | - | - | - | - | - | - | - |